The product is an insulating material coated with special modified epoxy resin in rhombic shape on electrical insulating paper. The product is widely used for interlayer insulation and turn to turn insulation of Oil-immersed power transformers. When in use, the coating layer begins to melt at a certain temperature during the drying process of the coil, resulting in adhesion. With the increase of temperature, it begins to solidify, so that the adjacent layers of the winding can be reliably bonded into a fixed unit.The adhesive strength of epoxy resin is enough to prevent the displacement of each layer of winding in case of short circuit, so as to ensure the long-term electrical and mechanical properties of the insulation structure. Because the resin coating of the insulating paper on the rhombic gel is in the shape of dots, it ensures the immersion of oil and the elimination of gas in the insulating material, effectively avoids corona and partial discharge, so as to ensure the safety and reliability of the insulating structure.
Item
Property
Unit
Requirement
Base material Thickness(mm)
0.08±0.005
0.13±0.007
0.18±0.010
0.38±0.020
0.50±0.030
1
Base material Density
g/m3
0.85 ~ 1.10
2
Coating thickness
μm
10 ~ 15
3
Moisture content
%
4.0 ~ 8.0
4
Oil absorption rate
%
≥60
5
Bond strength
RT
kpa
≥60
100℃±2℃
≥60
6
No-pollution oil of transformer
/
<0.001△tg0
7
Tensile Strength
MD
N/10mm
≥60
≥110
≥160
≥180
≥230
CD
N/10mm
≥30
≥50
≥70
≥80
≥100
8
Tear strength
MD
nN
≥450
≥900
≥1350
≥1500
≥2000
CD
≥500
≥1000
≥1500
≥1700
≥2300
9
Dielectric breakdown
In air
KV
≥0.88
≥1.37
≥2.00
≥2.10
≥2.25
In oil
≥4.40
≥7.00
≥9.00
≥9.80
≥11.50
10
Curing conditions
Heat to 90 ℃, hold for 3 hours, raise the temperature to 125 ℃, and hold for 6 hours